Paper properties

Property Value (SI) Value (US) Test method
Grammage 100 ± 3 g/m² 26.6 ± 0.8 17x22 - 500 lbs ISO 536
Thickness 82 ± 5 µm 3.23 ± 0.20 mils ISO 534
Moisture, PM 6.0 ± 0.5 % ISO 287
ISO Brightness C/2°, CS 92 ≥ 87 % ISO 2470
Opacity 90 ≥ 85 % ISO 2471
Gloss 75°, CS 78 ± 6 ISO 8254-1
Roughness PPS 10, CS 0.5 ≤ 1.0 µm ISO 8791-4
Tensile strength (MD) 4.6 ≥ 4.1 kN/m 26.3 ≥ 23.4 lbf/in ISO 1924-3
Tensile strength (CD) 2.9 ≥ 2.4 kN/m 16.6 ≥ 13.7 lbf/in ISO 1924-3
Tear strength (MD) 410 ≥ 330 mN 41.8 ≥ 33.7 gf ISO 1974
Tear strength (CD) 430 ≥ 350 mN 43.8 ≥ 35.7 gf ISO 1974
Unger oil absorption, RS 0.5 ≤ 1.3 g/m² SCAN-P37 (60 sec)
IGT surface strength, CS 0.9 ≥ 0.4 m/s ISO 3783